[1]齐丕骧,齐霖.铝合金挤压铸件缺陷概论[J].特种铸造及有色合金,2001(S1):104-107.
Qi Pixiang Qi Lin. Generality of the defects of aluminum alloy casting by squeeze-casting[J]. Special Casting & Nonferrous Alloys, 2001,(S1):104-107.
概要讨论了各种挤压铸造条件下
铝合金挤压铸件的缺陷(如:缩松、缩孔、夹渣、冷隔、浇不足、偏析、气孔及裂纹 等)形成机制、特征、影响因素及防止办法等。
In this paper
the defects of aluminum alloy casting by squeeze - casting ware discussed. The defects include shrinkage
entrapped slay
cold lap
misrun
segregation
and crack etc
they were formed in different squeeze - casting conditions. The mechanism and character and effect factors and avoidance ways were introduced.
挤压铸造铝合金缺陷
Squeezing-castingAluminum AlloyDefect