Black point defects in investment casting stainless parts were analyzed.Through adjusting gating system
setting filter screen at ingate to filter and purify liquid metal
and reducing ingate area or runner width
black point in the casting can be greatly eliminated.In addition
removal of residual wax should be completely cleaned
and rational deoxide operation should be noted in process of refinery and pouring.