Li Yanxi. Industrial Experiment for Li-Si Alloy Powder. [J]. Special Casting & Nonferrous Alloys (1):66-88(2004)DOI:
Industrial Experiment for Li-Si Alloy Powder
摘要
在熔炼温度为 75 0℃
熔炼时间为 1h
原料高纯金属锂过量 2 .5 %的情况下
用高纯金属锂和高纯硅为原料
成功地批量制备出w(Li) =44 %
w(Si) =5 6%的锂硅合金。锂硅合金经研磨粉碎、筛粉分级而成锂硅合金粉。
Abstract
Li-Si alloy containing 44%Li and 56%Si is produced successfully by smelting at high temperature 750 ℃ for 1 h with the raw materials of high pure Si and Li with expectant less w (Li) =2.5% during smelting. The Li-Si alloy has to be ground sieved and classified.