Liu Xiang-liang1, Tu Yiyou1, Jiang Jianqing1, et al. 5052 Alloy Ingot in Semi-continuous Casting. [J]. Special Casting & Nonferrous Alloys (10):789-790(2007)
Liu Xiang-liang1, Tu Yiyou1, Jiang Jianqing1, et al. 5052 Alloy Ingot in Semi-continuous Casting. [J]. Special Casting & Nonferrous Alloys (10):789-790(2007)DOI:
The effects of the friction force between crystalline and surface of the ingot
cooling water pressure on the quality of the 5052 alloy ingot have been examined. The microstructure of the subsurface under different processing was observed by a polarized light microscope
and the chemical compositions of the segregation area were detected by EDAX. The results indicate that the liquid aluminum breakout can be effectively eliminated by polishing crystalline
applying lubricant oil on the crystalline wall and increasing cooling water pressure during pouring. In addition
the surface macro-segregation can be obviously restrained by increasing the cooling pressure up to 0.20 MPa.