Heat Treatment Process and Properties of Al-7Si-0.3Mg-0.3Y Alloy
- “In the field of improving the mechanical properties of cast Al-7Si-0.3Mg-0.3Y alloy, researchers have determined through heat treatment and equipment analysis that the optimal process is 530 ℃× 6h+160 ℃× 11.5h, significantly improving the tensile strength and elongation of the alloy.”
- Vol. 45, Issue 1, Pages: 52-58(2025)
Published: 20 January 2025